Skip to content
Schmitz Metallographie GmbH

Schmitz-Metallographie GmbH

  • de
  • Homepage
  • Metallography Supplies
    • Cutting
    • Mounting
    • Grinding
    • Polishing
    • Etching
    • Equipment
    • Preparation Recipes
    • Training Courses
  • Diamond Polish
    • Polish Production
    • Diamond Slurry
    • Diamond Paste
    • Diamond Powder
    • Lubricant
    • Quality Control
  • Material Technology
    • Failure Analysis
    • Metallography
    • Scanning Electron Microscopy
    • Residual Stress Measurement
    • Corrosion
    • Material Testing
    • Mobile Analysis
  • Microstructure Database
  • News
  • Contact
    • About us
  • Visit Online-Shop

Corrosion Damages

banner-gdb-korrosionsschaden
Schmitz / Database / Corrosion Damages (43)
    • Additive Manufacturing (AM) (15)
    • Al-Base (72)
    • Cast Iron (49)
    • Co-Base (8)
    • Corrosion Damages (43)
    • Cu-Base (75)
    • Edge zone (40)
    • Failure Cases (60)
    • Fe-Base (343)
    • Fe-Heat Treatment Series (91)
    • Mg-Base (3)
    • Ni-Base (24)
    • Other (19)
    • Plastics (15)
    • SEM (99)
    • Ti-Base (10)
    • Zn-Base (5)
  • 1.4571 | X6CrNiMoTi17-12-2 Fatigue Corrosion Cracking - 021.4571 | X6CrNiMoTi17-12-2 Fatigue Corrosion Cracking
  • 1.4571 | X6CrNiMoTi17-12-2 Stress corrosion cracking
  • Carrying out a dezincification test according to DIN EN ISO 6509-1 - 01Carrying out a dezincification test according to DIN EN ISO 6509-1
  • Cavitation corrosion in a heating pipe
  • Cavitation corrosion in condensate collector tube - 2Cavitation corrosion in condensate collector tube
  • Corroded Heating Pipes Made from Construction Steel - 04Corroded Heating Pipes Made from Construction Steel
  • CuAl8 solder on S235JR, liquid metal induced stress corrosion cracking - 22CuAl8 solder on S235JR, liquid metal induced stress corrosion cracking
  • CuZn39Pb2 | CW612N Stress corrosion cracking in brass
  • CW509L | CuZn40 Stress corrosion cracking in alpha brass - 02CW509L | CuZn40 Stress corrosion cracking in alpha brass
  • CW510L | CuZn42 Dezincification test acc. to DIN EN ISO 6509-1 - 03CW510L | CuZn42 Dezincification test acc. to DIN EN ISO 6509-1
  • CW604N | CuZn37Pb0.5 Stress corrosion cracking
  • CW614N | CuZn39Pb3 Dezincification test according to DIN EN ISO 6509-1 - 01CW614N | CuZn39Pb3 Dezincification test according to DIN EN ISO 6509-1
  • CW617N | CuZn40Pb2 Dezincification on ball valve shut-off valve - 08CW617N | CuZn40Pb2 Dezincification on ball valve shut-off valve
  • CW617N | CuZn40Pb2 Stress corrosion cracking - 01CW617N | CuZn40Pb2 Stress corrosion cracking
  • Dezincification of a siphon made of CW506L | CuZn33 | C26800 - 03Dezincification of a siphon made of CW506L | CuZn33 | C26800
  • Dezincification of an α-β-MessingDezincification of an α-β-Messing
  • Dezincification test of CW626N | CuZn33Pb1.5AlAs - 1Dezincification test of CW626N | CuZn33Pb1.5AlAs
  • EN AC-42200 | AlSi7Mg0,6 (T6) Sand casting, vibration corrosion cracking - 04EN AC-42200 | AlSi7Mg0,6 (T6) Sand casting, vibration corrosion cracking
  • EN AW-2007 | AlCu4PbMgMn | 3.1645 - 05EN AW-2007 | AlCu4PbMgMn | 3.1645
  • EN AW-5019 | AlMg5 intergranular corrosion - 03EN AW-5019 | AlMg5 intergranular corrosion
  • Erosion corrosion on heating pipe - 1Erosion corrosion on heating pipe
  • Exfoliation corrosion in EN AW-7075 T6 | AlZn5.5MgCu | AA7075 - 3Exfoliation corrosion in EN AW-7075 T6 | AlZn5.5MgCu | AA7075
  • Galvanic corrosion (bimetallic corrosion) of a hot water pipe - 04Galvanic corrosion (bimetallic corrosion) of a hot water pipe
  • Gaphite corrosion (spongiosis) lamellar gray cast iron - 04Gaphite corrosion (spongiosis) lamellar gray cast iron
  • Graphite corrosion (spongiosis) in a degenerated nodular graphite iron - 02Graphite corrosion (spongiosis) in a degenerated nodular graphite iron
  • High-temperature corrosion in a furnace hatch made of 1.4460 | X3CrNiMo27-5-2 | AISI 329 | S32900High-temperature corrosion in a furnace hatch made of 1.4460 | X3CrNiMo27-5-2 | AISI 329 | S32900
  • Intergranular corrosion in 1.4828 | X15CrNiSi20-12 | AISI 309 | S30900 - 03Intergranular corrosion in 1.4828 | X15CrNiSi20-12 | AISI 309 | S30900
  • Pitting corrosion attack on Aluminium by foreign metallic particlesPitting corrosion attack on Aluminium by foreign metallic particles
  • Pitting corrosion in 1.4305 | X8CrNiS18-9 | AISI 303 | S30300 after 24h use in “stale water”Pitting corrosion in 1.4305 | X8CrNiS18-9 | AISI 303 | S30300 after 24h use in “stale water”
  • Shallow pitting/crevice corrosion in 1.4509 | X2CrTiNb18 | AISI 441 | S43940 - 4Shallow pitting/crevice corrosion in 1.4509 | X2CrTiNb18 | AISI 441 | S43940
  • Shallow pitting/crevice corrosion in 1.4521 | X2CrMoTi18-2 | AISI 444 | S44400 - 03Shallow pitting/crevice corrosion in 1.4521 | X2CrMoTi18-2 | AISI 444 | S44400
  • Stress corrosion attack in α brassStress corrosion attack in α brass
  • Stress corrosion cracking (chlorine-induced) in CrNi steelStress corrosion cracking (chlorine-induced) in CrNi steel
  • Stress corrosion cracking (chlorine-induced) in high-alloyed CrNi steel 1.4404 | X2CrNiMo17-12-2 | AISI 316L | S31603Stress corrosion cracking (chlorine-induced) in high-alloyed CrNi steel 1.4404 | X2CrNiMo17-12-2 | AISI 316L | S31603
  • Stress corrosion cracking (molten metal induced) | hot-dip galvanisation - 11Stress corrosion cracking (molten metal induced) | hot-dip galvanisation
  • Stress corrosion cracking in a catastrophically corroded component of a heat exchangerStress corrosion cracking in a catastrophically corroded component of a heat exchanger
  • Stress corrosion cracking in welded heat exchanger tube made of CuZn - 04Stress corrosion cracking in welded heat exchanger tube made of CuZn
  • Stress corrosion cracking on brass CW617N | CuZn40Pb2 | C37700 - 1Stress corrosion cracking on brass CW617N | CuZn40Pb2 | C37700
  • Stress corrosion cracking on brass screw connection CW601N | CuZn35Pb2 | C34200 - 02Stress corrosion cracking on brass screw connection CW601N | CuZn35Pb2 | C34200
  • Stress corrosion cracking, solder brittleness of 1.0038 | S235JR | K01500 with CuAlNi2 solder - 4Stress corrosion cracking, solder brittleness of 1.0038 | S235JR | K01500 with CuAlNi2 solder
  • Stress corrosion damage of a heat exchanger tube 1.4301 | X5CrNi18-10 | AISI 304 | S30400Stress corrosion damage of a heat exchanger tube 1.4301 | X5CrNi18-10 | AISI 304 | S30400
  • Surface and pitting corrosion in a water pipe - 1Surface and pitting corrosion in a water pipe
  • Surface corrosion on cold water pipe - 2Surface corrosion on cold water pipe

Metallography Supplies

  • Cutting
  • Mounting
  • Grinding
  • Polishing
  • Etching
  • Equipment
  • Preparation Recipes
  • Training Courses

Diamond Polish

  • Polish Production
  • Diamond Slurry
  • Diamond Paste
  • Diamond Powder
  • Lubricant
  • Quality Control

Material Technology

  • Failure Analysis
  • Metallography
  • Scanning Electron Microscopy
  • Residual Stress Measurement
  • Corrosion
  • Material Testing
  • Mobile Analysis

Downloads

  • Preparation Recipes
  • Safety Data Sheets

Contact

Schmitz-Metallographie GmbH
Kaiserstraße 100
52134 Herzogenrath
Germany

Phone: +49 2407 568296-0
Fax: +49 2407 568296-9
E-Mail: info@schmitz-metallographie.de

  • Contact
  • Imprint
  • Data Privacy
  • Right of Withdrawal
© 2025 Schmitz-Metallographie GmbH