692 Case studies, 4884 figures (Updated: 21.12.2024)
- Additive Manufacturing (AM) (15)
- Al-Base (72)
- Cast Iron (49)
- Co-Base (8)
- Corrosion Damages (43)
- Cu-Base (75)
- Edge zone (39)
- Failure Cases (60)
- Fe-Base (333)
- Fe-Heat Treatment Series (91)
- Mg-Base (3)
- Ni-Base (24)
- Other (19)
- Plastics (15)
- SEM (99)
- Ti-Base (10)
- Zn-Base (5)
We have already collected more than 690 case studies and failure cases for you in our structures database. Sorted by material, you are sure to find the microstructure you are looking for.
Do you have any other interesting materials or coatings?
You are welcome to send them to us. We will prepare them and include the cases in our database.
Pictures and graphics are subject to the copyright of Schmitz-Metallographie GmbH.
Latest case studies
- Magnetic material Manganese-zinc ferrites (MnZn+Fe2O4)
- 1.1191 | C45E +QW +T Hardened and tempered (quenchant: water)
- EN AW-2011 | AlCu6BiPb
- 1.7131 | 16MnCr5 +QW +T Hardened and tempered (quenchant: water)
- Ir-MMO coatings on titanium anodes
- CuAl8 solder on S235JR, liquid metal induced stress corrosion cracking
- 1.8519 | 31CrMoV9 +QT
- 1.7225 | 42CrMo4 +QO +T Hardened and tempered (quenchant: oil)
- GJS-1400-1 | ADI | Fracture appearance in tensile test
- 1.4571 | X6CrNiMoTi17-12-2 Fatigue Corrosion Cracking
- 1.2343 | X38CrMoV5-1 +QT
- 1.2067 | 102Cr6 +QW +T Hardened and tempered (tempering temperature: 210 °C)