697 Case studies, 4880 figures (Updated: 24.01.2025)
- Additive Manufacturing (AM) (15)
- Al-Base (72)
- Cast Iron (49)
- Co-Base (8)
- Corrosion Damages (43)
- Cu-Base (75)
- Edge zone (40)
- Failure Cases (60)
- Fe-Base (337)
- Fe-Heat Treatment Series (91)
- Mg-Base (3)
- Ni-Base (24)
- Other (19)
- Plastics (15)
- SEM (99)
- Ti-Base (10)
- Zn-Base (5)
We have already collected more than 690 case studies and failure cases for you in our structures database. Sorted by material, you are sure to find the microstructure you are looking for.
Do you have any other interesting materials or coatings?
You are welcome to send them to us. We will prepare them and include the cases in our database.
Pictures and graphics are subject to the copyright of Schmitz-Metallographie GmbH.
Latest case studies
CW103C | CuCo1Ni1Be
EN-GJS-800-2 | 5.3301 Graphite classification and fracture appearance in tensile test
EN-GJS-600-3 | 5.3201 | Graphite classification and fracture appearance in tensile test
EN-GJS-500-7 | 5.3200 | Graphite classification and fracture appearance in tensile test
EN-GJS-500-14 | 5.3109 | Graphite classification and fracture appearance in tensile test
EN-GJS-450-10 | 5.3107 | Graphite classification and fracture appearance in tensile test
Titanium Grade 23 | Ti6Al4V ELI | PF -45/+15 µm
Titanium Grade 23 | Ti6Al4V ELI | PF -45/+15 µm | VED 117 J/mm³ | BUR 11 cm³/h
Titanium Grade 23 | Ti6Al4V ELI | PF -45/+15 µm | VED 50 J/mm³ | BUR 9 cm³/h
Titanium Grade 23 | Ti6Al4V ELI | PF -45/+15 µm | VED 58 J/mm³ | BUR 21.6 cm³/h
EN-GJS-400-15 | 5.3106 | EN-JS1030 Graphite classification and fracture appearance in tensile tests