We have already collected more than 690 case studies and failure cases for you in our structures database. Sorted by material, you are sure to find the microstructure you are looking for.
Do you have any other interesting materials or coatings?
You are welcome to send them to us. We will prepare them and include the cases in our database.
Pictures and graphics are subject to the copyright of Schmitz-Metallographie GmbH.
Latest case studies
- 1.2312 | 40CrMnMoS8-6 +QT
- EN-GJL-250 (+P) | 5.1301 Increased phosphorus content, graphite classification and fracture appearance in tensile test
- 1.7182 | 27MnCrB5-2 case hardened
- 1.4404 | X5CrNoMo17-12-2 | PF -45/+15 µm | VED 41,67 J/mm³ | BUR 21,60 cm³/h
- 1.4404 | X5CrNoMo17-12-2 | PF -45/+15 µm | VED 27,78 J/mm³ | BUR 25,92 cm³/h
- 1.4404 | X5CrNoMo17-12-2 | PF -45/+15 µm | VED 74,4 J/mm³ | BUR 12,10 cm³/h
- 1.4404 | X5CrNoMo17-12-2 | PF -45/+15 µm
- Graphite degeneration: White irradiation in GJS | Damage case with brittle cleavage fracture
- EN-GJL-250 | 5.1301 Graphite classification and fracture appearance in the tensile test
- 1.0577 | S355J2 +N
- 1.7182 | 27MnCrB5-2 +QT
- 1.0986 | S550 +MC