701 Case studies, 4919 figures (Updated: 27.02.2025)
- Additive Manufacturing (AM) (15)
- Al-Base (72)
- Cast Iron (49)
- Co-Base (8)
- Corrosion Damages (43)
- Cu-Base (75)
- Edge zone (40)
- Failure Cases (60)
- Fe-Base (341)
- Fe-Heat Treatment Series (91)
- Mg-Base (3)
- Ni-Base (24)
- Other (19)
- Plastics (15)
- SEM (99)
- Ti-Base (10)
- Zn-Base (5)
We have already collected more than 700 case studies and failure cases for you in our structures database. Sorted by material, you are sure to find the microstructure you are looking for.
Do you have any other interesting materials or coatings?
You are welcome to send them to us. We will prepare them and include the cases in our database.
Pictures and graphics are subject to the copyright of Schmitz-Metallographie GmbH.
Latest case studies
C67300
EN AW-2007 | AlCu4PbMgMn | 3.1645
M50NiL (Spec) | AMS 6278D, formerly 1.3590
CW614N | CuZn39Pb3 Dezincification test according to DIN EN ISO 6509-1
1.4545 | X5CrNiCu15-5 +AT
CW510L | CuZn42 Dezincification test acc. to DIN EN ISO 6509-1
1.3551 | 80MoCrV42-16 +QT
Carrying out a dezincification test according to DIN EN ISO 6509-1
CW004A | Cu-ETP
1.1121 | C10E +N (furnace cooling)
CW617N | CuZn40Pb2 Dezincification on ball valve shut-off valve
1.8519 | 31CrMoV9 ChromOx