697 Case studies, 4880 figures (Updated: 24.01.2025)
- Additive Manufacturing (AM) (15)
- Al-Base (72)
- Cast Iron (49)
- Co-Base (8)
- Corrosion Damages (43)
- Cu-Base (75)
- Edge zone (40)
- Failure Cases (60)
- Fe-Base (337)
- Fe-Heat Treatment Series (91)
- Mg-Base (3)
- Ni-Base (24)
- Other (19)
- Plastics (15)
- SEM (99)
- Ti-Base (10)
- Zn-Base (5)
We have already collected more than 690 case studies and failure cases for you in our structures database. Sorted by material, you are sure to find the microstructure you are looking for.
Do you have any other interesting materials or coatings?
You are welcome to send them to us. We will prepare them and include the cases in our database.
Pictures and graphics are subject to the copyright of Schmitz-Metallographie GmbH.
Latest case studies
Bolt 8.8 with Fatigue Fracture
1.7225 | 42CrMo4 +N Normalised at 850 °C (furnace cooling)
1.7131 | 16MnCr5 +N Normalised at 950 °C (furnace cooling)
1.1221 | C60E +N Normalised at 850 °C (furnace cooling)
1.0535 | C55 +N Normalised at 850 °C (furnace cooling)
1.1191 | C45E +N Normalised at 850 °C (cooled with compressed air)
1.0501 | C35 +N Normalised at 900 °C (furnace cooling)
1.0401 | C15 +N Normalised at 950 °C (furnace cooling)
1.1191 | C45E +N Normalised at 850 °C (furnace cooling)
1.4840 | GX15CrNi25-20
1.3243 | HS6-5-2-5 +QA+T nitrided
1.3243 | HS6-5-2-5 +QA+T