706 Case studies, 4937 figures (Updated: 17.03.2025)
- Additive Manufacturing (AM) (15)
- Al-Base (72)
- Cast Iron (49)
- Co-Base (8)
- Corrosion Damages (43)
- Cu-Base (75)
- Edge zone (41)
- Failure Cases (60)
- Fe-Base (346)
- Fe-Heat Treatment Series (91)
- Mg-Base (3)
- Ni-Base (24)
- Other (19)
- Plastics (15)
- SEM (99)
- Ti-Base (10)
- Zn-Base (5)
We have already collected more than 700 case studies and failure cases for you in our structures database. Sorted by material, you are sure to find the microstructure you are looking for.
Do you have any other interesting materials or coatings?
You are welcome to send them to us. We will prepare them and include the cases in our database.
Pictures and graphics are subject to the copyright of Schmitz-Metallographie GmbH.
Latest case studies
Sintered steel Sint-C 39 carbonitrided +QT
CW604N | CuZn37Pb0.5 Stress corrosion cracking
CW604N | CuZn37Pb0.5
Sintered steel Sint-C 39 normalised
CW724R | CuZn21Si3P | Cuphin in as-cast condition
1.1248 | C75S +I Grinding burn
CW718R | CuZn39Mn1AlPbSi
1.7379 | G17CrMo-9-10 Tensile test specimen
1.0552 | S460J2
EN AW-6061 | AlMg1SiCu
EN GJSA-XNi35
EN AW-5754 | AlMg3