697 Case studies, 4880 figures (Updated: 24.01.2025)
- Additive Manufacturing (AM) (15)
- Al-Base (72)
- Cast Iron (49)
- Co-Base (8)
- Corrosion Damages (43)
- Cu-Base (75)
- Edge zone (40)
- Failure Cases (60)
- Fe-Base (337)
- Fe-Heat Treatment Series (91)
- Mg-Base (3)
- Ni-Base (24)
- Other (19)
- Plastics (15)
- SEM (99)
- Ti-Base (10)
- Zn-Base (5)
We have already collected more than 690 case studies and failure cases for you in our structures database. Sorted by material, you are sure to find the microstructure you are looking for.
Do you have any other interesting materials or coatings?
You are welcome to send them to us. We will prepare them and include the cases in our database.
Pictures and graphics are subject to the copyright of Schmitz-Metallographie GmbH.
Latest case studies
Stress corrosion cracking (chlorine-induced) in high-alloyed CrNi steel 1.4404 | X2CrNiMo17-12-2 | AISI 316L | S31603
Stress corrosion cracking (chlorine-induced) in CrNi steel
Stress corrosion cracking on brass screw connection CW601N | CuZn35Pb2 | C34200
Shallow pitting/crevice corrosion in 1.4509 | X2CrTiNb18 | AISI 441 | S43940
Shallow pitting/crevice corrosion in 1.4521 | X2CrMoTi18-2 | AISI 444 | S44400
Stress corrosion cracking on brass CW617N | CuZn40Pb2 | C37700
Stress corrosion cracking in welded heat exchanger tube made of CuZn
Stress corrosion attack in α brass
Stress corrosion cracking in a catastrophically corroded component of a heat exchanger
Stress corrosion damage of a heat exchanger tube 1.4301 | X5CrNi18-10 | AISI 304 | S30400
Gaphite corrosion (spongiosis) lamellar gray cast iron
Graphite corrosion (spongiosis) in a degenerated nodular graphite iron