697 Case studies, 4880 figures (Updated: 24.01.2025)
- Additive Manufacturing (AM) (15)
- Al-Base (72)
- Cast Iron (49)
- Co-Base (8)
- Corrosion Damages (43)
- Cu-Base (75)
- Edge zone (40)
- Failure Cases (60)
- Fe-Base (337)
- Fe-Heat Treatment Series (91)
- Mg-Base (3)
- Ni-Base (24)
- Other (19)
- Plastics (15)
- SEM (99)
- Ti-Base (10)
- Zn-Base (5)
We have already collected more than 690 case studies and failure cases for you in our structures database. Sorted by material, you are sure to find the microstructure you are looking for.
Do you have any other interesting materials or coatings?
You are welcome to send them to us. We will prepare them and include the cases in our database.
Pictures and graphics are subject to the copyright of Schmitz-Metallographie GmbH.
Latest case studies
Stellite 20 | Centrifugally casting
Co-base Alloy | Valve seat ring
WC-Co Weld metal
WC-17%Co
AZ91D | EN_MC MgAl9Zn1 | M11916
MgZnAl casting alloy
Wormhole
ZL0400 | ZnAl4
Aramid fibers
Balloon catheter with active ingredient coating
Basalt fibers
Carbon fiber reinforced plastic component from the racing sector