- Additive Manufacturing (AM) (15)
- Al-Base (70)
- Cast Iron (48)
- Co-Base (8)
- Corrosion Damages (43)
- Cu-Base (75)
- Edge zone (38)
- Failure Cases (60)
- Fe-Base (318)
- Fe-Heat Treatment Series (85)
- Mg-Base (3)
- Ni-Base (23)
- Other (16)
- Plastics (15)
- SEM (99)
- Ti-Base (10)
- Zn-Base (5)
We have already collected more than 660 case studies and failure cases for you in our structures database. Sorted by material, you are sure to find the microstructure you are looking for.
Do you have any other interesting materials or coatings?
You are welcome to send them to us. We will prepare them and include the cases in our database.
Pictures and graphics are subject to the copyright of Schmitz-Metallographie GmbH.
Latest case studies
EN-GJL-200 | 5.1300 Overload fracture in gray cast iron
EN AC-43000 | AlSi10Mg die casting, Cold flow marks
Hydrogen embrittlement in locking washer
WEA White Etching Area
CC499K | CuSn5Zn5Pb2-C Brass fitting with hot crack
CA103 | CuAl10Fe3| C62300
CW021A | Cu-HCP | C10800 Pure copper
C61000 | CuAl6Ni2 Extrusion alloy
Hardening crack on a screw
EN AW-2007 | AlCu4PbMg | AA2007 Cracks due to cumulative and coarse precipitations
EN AC-42200 | AlSi7Mg0,6 Fatigue fracture vs. overload fracture
1.0143 | S275J0 Steel beam with fire damage