697 Case studies, 4880 figures (Updated: 24.01.2025)
- Additive Manufacturing (AM) (15)
- Al-Base (72)
- Cast Iron (49)
- Co-Base (8)
- Corrosion Damages (43)
- Cu-Base (75)
- Edge zone (40)
- Failure Cases (60)
- Fe-Base (337)
- Fe-Heat Treatment Series (91)
- Mg-Base (3)
- Ni-Base (24)
- Other (19)
- Plastics (15)
- SEM (99)
- Ti-Base (10)
- Zn-Base (5)
We have already collected more than 690 case studies and failure cases for you in our structures database. Sorted by material, you are sure to find the microstructure you are looking for.
Do you have any other interesting materials or coatings?
You are welcome to send them to us. We will prepare them and include the cases in our database.
Pictures and graphics are subject to the copyright of Schmitz-Metallographie GmbH.
Latest case studies
1.7102 | 54SiCr6 +QT
1.3505 | 100Cr6 +QT
AA-6020 as cast
1.4571 | X6CrNiMoTi17-12-2 Stress corrosion cracking
1.2067 | 102Cr6 Incomplete martensitic transformation (2)
1.4864 | X12NiCrSi35-16
1.0338 | DC04 +C340 (cold rolled)
2.4819 | NiMo16Cr15W | Alloy C-276
1.2067 | 102Cr6 +N Normalized at 840 °C (furnace cooling)
1.2067 | 102Cr6 +QW +T Annealed on cementite network, superheat hardened and tempered
"BiSn34" Lead-free alloy for "lead casting on New Year's Eve"
EN AC-43500 | AlSi10MnMg Cold run and hot crack