697 Case studies, 4880 figures (Updated: 24.01.2025)
- Additive Manufacturing (AM) (15)
- Al-Base (72)
- Cast Iron (49)
- Co-Base (8)
- Corrosion Damages (43)
- Cu-Base (75)
- Edge zone (40)
- Failure Cases (60)
- Fe-Base (337)
- Fe-Heat Treatment Series (91)
- Mg-Base (3)
- Ni-Base (24)
- Other (19)
- Plastics (15)
- SEM (99)
- Ti-Base (10)
- Zn-Base (5)
We have already collected more than 690 case studies and failure cases for you in our structures database. Sorted by material, you are sure to find the microstructure you are looking for.
Do you have any other interesting materials or coatings?
You are welcome to send them to us. We will prepare them and include the cases in our database.
Pictures and graphics are subject to the copyright of Schmitz-Metallographie GmbH.
Latest case studies
1.2241 | 51CrMnV4 Bainitized
1.2067 | 102Cr6 +QW +T Annealed on cementite network, hardened and tempered (quenchant: water)
1.0330 | DC01 +LC (soft annealed and slightly re-rolled)
1.2067 | 102Cr6 +QO +T Hardened and tempered at 150 °C (quenchant: oil)
1.2067 | 102Cr6 +QO +T Hardened and tempered at 180 °C (quenchant: oil)
1.2067 | 102Cr6 +QO +T Hardened and tempered at 150 °C (quenchant: oil)
1.2067 | 102Cr6 +QO +T Hardened and tempered (quenchant: oil)
1.2067 | 102Cr6 Annealed on cementite network at 950 °C
1.3401 | X120Mn12 Strain-hardened
Diamond honing stone is fake
1.0503 | C45 Incorrect induction hardened
1.0501 | C35 Inductively hardened